"He who marches out of step hears another drum." ~ Ken Kesey
So why no Fixer N?? Do you mean it isn't necessary with the CCI bases? I thought it was designed to enhance wash fastness, so I've been using it in all my WB Pigmented Discharge, and straight WB jobs. I don't use it in straight discharge jobs, meaning non-pigmented.
just to add, we ran into this same issue with matsui white, but we had more of a stencil problem than ink. Our emulsion wasn't exposed properly. we went from an sbq to a dual cure and we hadn't hit the correct expoure time, so that was creating a bit of havoc for us with the dreaded "zombie skin". I know exactly what you are talking about. I bet the temp in the shop didn't help us either. I'll watch the air temp and see where we are when this issue comes up. Hopefully I can try some cci stuff and not worry about it at all.
Don't forget their Hardener X for long runs on the emulsion. Also CCI has pigment kits for $75. Base, PC, and ZFS is all you need......none of that other stuff. Thin with water. Formulas are taken straight from the Pantone books