Author Topic: I-Image STE emulsion for discharge  (Read 5779 times)

Offline Frog

  • Administrator
  • Ludicrous Speed Member
  • *****
  • Posts: 13980
  • Docendo discimus
Re: I-Image STE emulsion for discharge
« Reply #15 on: January 22, 2018, 09:36:55 AM »
Do test coating 1/1,1/2,2/1,2/2 etc  and then expose a design that will allow you to test different parts of your screen for proper eom.

Go with the coating technique that proves the best for you.

When I used the PHU I coated my 150s 2/1 with a monster max scoop coater and everything higher 1/1.

Generally, doesn't one need more strokes to coat higher mesh counts since the mesh naturally holds less?
That rug really tied the room together, did it not?


Offline AAMike

  • Full Member
  • ***
  • Posts: 207
Re: I-Image STE emulsion for discharge
« Reply #16 on: January 22, 2018, 11:29:20 AM »
Will do. Thanks fellas.

Offline Colin

  • !!!
  • Gonzo Member
  • ******
  • Posts: 1610
  • Ink and Chemical Product Manager
Re: I-Image STE emulsion for discharge
« Reply #17 on: January 22, 2018, 02:55:44 PM »
Do test coating 1/1,1/2,2/1,2/2 etc  and then expose a design that will allow you to test different parts of your screen for proper eom.

Go with the coating technique that proves the best for you.

When I used the PHU I coated my 150s 2/1 with a monster max scoop coater and everything higher 1/1.

Generally, doesn't one need more strokes to coat higher mesh counts since the mesh naturally holds less?

With thinner emulsions yes.  That has been my experience.

Both the PHU and the T9 are thicker bodied.  So if I tried to go 2/1 I would be printing HD sim process ;)
Been in the industry since 1996.  5+ years with QCM Inks.  Been a part of shops of all sizes and abilities both as a printer and as an Artist/separator.  I am now the Ink and Chemical Product Manager at Ryonet.