got my units installed and the tech is coming today for the i-Image.
couple of questions.
I use Ulano blue and will only be using 3 mesh types: 150S, 225S, 305
I typically coat my 150s with a 1print/2 ink side and the higher mesh with a 1/1
is this optimal? or should I be going 1/2 on everything? Also, anyone have burn times for this setup?
Probably 4 second exposure time, that's what we have with Ulano Orange.
Do you find the Blue holds enough resolution on 225S, 305? I ask because we use a dual cure for our higher meshes.
For the coating you will almost certainly only need 1/1 for the 150S at least, sharp edge 2/2 for 225S / 305 maybe....but you could just go slower and probably achieve the right EOM.
I didn't see the solids content and don't use Blue but it shouldn't be too different from Orange I think.
Good luck, those are great pieces of equipment.