"He who marches out of step hears another drum." ~ Ken Kesey
Ok using Kaeser gold foil with wilflex foil hd 2. Had problems till we went 380 on our stahls press and 13-15 seconds. I am having more problems with corner on the tip of the crown or main no coming out and have to repress with extra foil. What am i doing wrong??? tried virus adhesive no luck at all. No the foil in the rest is coming out? Using sanmar triblend shirts and t-hoodies. Also in about 30-45% humidty-Swamp cooler.Help, ideas?Thanks,Shane
Quote from: cbjamel on June 14, 2018, 09:41:48 PMOk using Kaeser gold foil with wilflex foil hd 2. Had problems till we went 380 on our stahls press and 13-15 seconds. I am having more problems with corner on the tip of the crown or main no coming out and have to repress with extra foil. What am i doing wrong??? tried virus adhesive no luck at all. No the foil in the rest is coming out? Using sanmar triblend shirts and t-hoodies. Also in about 30-45% humidty-Swamp cooler.Help, ideas?Thanks,ShaneI'm far from a foil expert, but i feel like that temp is way to hot. For us the key to foil is letting it cool. Not like waiting 10 seconds cool, like doing the whole run, and letting it cool, then peeling it off.