TSB

screen printing => Screen Making => Topic started by: noortrd on January 09, 2014, 08:03:21 AM

Title: hxt with hardener
Post by: noortrd on January 09, 2014, 08:03:21 AM
We exposed hxt on 2k light around 4 minute.  After we use hardener. But its runs only 50 piece on water base. Can we also use diazo and than hardener?. Or only use diazo with no hardener.
Title: Re: hxt with hardener
Post by: Printficient on January 09, 2014, 08:07:51 AM
What is your procedure for applying the hardener?
Title: Re: hxt with hardener
Post by: noortrd on January 09, 2014, 08:29:58 AM
with the help on sponge.
Title: Re: hxt with hardener
Post by: Colin on January 09, 2014, 12:43:28 PM
How long are you leaving the hardener on the screen before printing?

What is the humidity of your screens/screen storage before exposure?

Are you post exposing?

Do your waterbase inks have solvents in them?