Opportunity is missed by most people because it is dressed in overalls and looks like work. - Thomas Edison
Well, I just put a bullet proof screen on the press, no regi marks, post exposed, blockout, post expose, hardener, post expose in the sun, no tape on the shirt side, and it took 200 shirts for the emulsion to give way. Is anyone using Jantex Sweet? I've ran several 300-400 piece jobs without doing this much to the screens without any emulsion failure and now this is the second big job I've done with just the Jantex Sweet base with plastisol on top that has failed. I'm at a loss. I don't know if I can do anything else to a screen with the time constraints I have.
But I've also been told great things about the HVP and nobody has really had this type of problem or at least this severe yet here I am, having one of the worst days we've ever had. I know guys that have gotten a few thousand shirts with this emulsion without diazo without a breakdown. Something major is going on and I can't really figure it out.