The jacket is 90% nylon and 10% spandex. I'm thinking of just adding catalyst to some white plastisol and calling it good. Only question is: should I PFP or just get a nice double stroke down?
Endurance Plus white with 3% 900 series Catalyst. I double stroked but it may have looked a bit sharper if I would have just done one solid hit. I hit it with a heat gun a bit just to boost its cure time until it was very hot/dry to the touch. All Carhartt garments came out unscathed