I almost gave up today as I was recycling some screens we used during the week. All coated with CCI WR-14 all 330-S. First in the dip tank, not much luck getting the emulsion off, then a round of high concentrated Gem-Zyme, which helped but was far from the result I hoped for. I think I spend around 5 minuted per screen probably more to get the emulsion off, far from perfect though. It would have almost been faster to stretch new mesh on those roller frames instead of wasting all this time on trying to recycle them. Is there anything we can do to speed up the whole process, I can`t recall ever having such problems with any other emulsion. There wasn`t even any hardener used on those screens.