"He who marches out of step hears another drum." ~ Ken Kesey
Murakami HVP with 8gs of diazo, harden with MS Hardener.Dry and expose completely, post expose, dry well, Apply MS hardener throw in sun for an hour.Impervious to wb and discharge.
Ive stated this a million times, you haaaaaaaaaaave to give this emulsion a long exposure, Not just the the ole, no slim good to go.
To answer Frog while I am it here is a step test procedure to try:http://murakamiscreen.com/wp-content/uploads/2012/07/Step-Test-Instructions.pdfAlMurakami Screen.323.697.4334
Some guys swear by murikami hvp, for us, it was theeeee worst emulsion we tried in our system. Others love CP tex, didn't work for us either.